Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 4.69 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 4.69 GPa
680 ksi
ASTM D790
PolyOne Stat-Tech™ AS-08CF/000 Acrylonitrile Butadiene Styrene (ABS)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Flexural Modulus 4.69 GPa
680 ksi
ASTM D790
PolyOne Stat-Tech™ AS-08CF/000 UV FR V0 Acrylonitrile Butadiene Styrene (ABS)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Flexural Modulus 4.69 GPa
680 ksi
ASTM D790
Polymer Resources PC/TP-GP2-G20 PC/Polyester Alloy, 20% Glass Reinforced
Excellent Chemical Resistance, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information p..
Flexural Modulus 4.69 GPa
680 ksi
ASTM D790
PTS Trimid® N66-G13HL 13% Glass Fiber Reinforced Heat Stabilized, Lubed Nylon 6/6
Information provided by Polymer Technology and Services, LLC (PTS).
Flexural Modulus 4.69 GPa
680 ksi
ASTM D790
Polymer Resources PC/TP-GP2-G20 PC Polyester, Excellent Chemical Resistance, 20% Glass Filled  (Unverified
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Flexural Modulus 4.69 GPa
680 ksi
ASTM D790
PolyOne Edgetek® AS-20GF/000 FR Acrylonitrile Butadiene Styrene (ABS), Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Flexural Modulus 4.69 GPa
680 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP MX06402H PP
LNP* THERMOCOMP* MX06402H is a compound based on Polypropylene resin containing 20% Glass Fiber. Added features of this material include: Heat Stabilized, Low Extractable.
Flexural Modulus 4.69 GPa
680 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP RB006 PA 66
LNP* THERMOCOMP* RB006 is a compound based on Nylon 66 resin containing 30% Glass Bead.
Flexural Modulus 4.69 GPa
680 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP RB006 PA 66 (Asia Pacific)
LNP* Thermocomp* RB006 is a compound based on Nylon 66 resin containing Glass Bead.
Flexural Modulus 4.69 GPa
680 ksi
ASTM D790
A. Schulman SCHULADUR® A GF10 10% Glass Fiber Reinforced PBT
Information provided by A. Schulman.
Flexural Modulus 4.69 GPa
680 ksi
ASTM D790
Chase Plastics CP Pryme® N310L (Dry) Nylon 6, 10% Glass Fiber Reinforced, Lubricated, Recycled Content
Features: LubricatedRecycled contentForm: PelletsInformation provided by Chase Plastics.
Flexural Modulus 4.69 GPa
680 ksi
ASTM D790
Chase Plastics CP Pryme® N340MGL (COND, 50% RH) Nylon 6 (Utility Grade), 40% Mineral/Glass Fiber Reinforced, Internally Lubricated
Information provided by Chase Plastics.
Flexural Modulus 4.69 GPa
680 ksi
ASTM D790
A. Schulman SCHULADUR® A GF10 10% Glass Fiber Reinforced PBT
Information provided by A. Schulman.
Flexural Modulus 4.69 GPa
680 ksi
ASTM D790
A. Schulman SCHULADUR® A GF10 10% Glass Fiber Reinforced PBT
Information provided by A. Schulman.
Flexural Modulus 4.69 GPa
680 ksi
ASTM D790
A. Schulman SCHULADUR® A GF10 10% Glass Fiber Reinforced PBT
Information provided by A. Schulman.
Flexural Modulus 4.69 GPa
680 ksi
ASTM D790
A. Schulman SCHULADUR® A GF10 10% Glass Fiber Reinforced PBT
Information provided by A. Schulman.
Flexural Modulus 4.69 GPa
680 ksi
ASTM D790
A. Schulman SCHULADUR® A GF10 10% Glass Fiber Reinforced PBT
Information provided by A. Schulman.
Flexural Modulus 4.69 GPa

@Temperature 120 °C
680 ksi

@Temperature 248 °F
ASTM Test
BASF Petra® 140 45% Glass Filled PET
Petra 140 is a 45% glass reinforced injection molding polyethylene terephthalate (PET) offering an increased level of strength, stiffness, high temperature performance and dimensional stability. Ex..
Flexural Modulus 4.69 - 6.07 GPa
680 - 880 ksi
Bulk Molding Compounds BMC A50-EG Low Glass, Encapsulation Grade Molding Compound
BMC A50-EG is a low glass, encapsulation grade material. It is well suited for injection, transfer or compression molding of intricate parts. Typical applications are motor armatures and coils.Inf..
Flexural Modulus 4.69 GPa
680 ksi
ASTM D790
Asahi Kasei Thermylene® P6-35FM-1309 35% Glass and Mineral Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
Flexural Modulus 4.69 - 4.69 GPa

@Temperature 120 - 120 °C
680 - 680 ksi

@Temperature 248 - 248 °F
Average value: 4.69 GPa Grade Count:1
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% ..