Mechanical Properties Metric English Comments
Flexural Modulus 4.68 GPa
679 ksi
ISO 178
FKuR Kunststoff Bio-Flex® S 9533 Compostable PLA Blend
The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta..
Flexural Modulus 4.68 GPa
679 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Valox® EH7020HF PBT+PET
Valox EH7020HF is a mineral filled PBT/PET that offers good surface appearance, high flow and good heat performance. EH7020HF was developed for automotive bezel application that requires basecoat + ..
Flexural Modulus 4.68 GPa
679 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Valox® EH7020HF PBT+PET (Asia Pacific)
Valox EH7020HF is a mineral filled PBT/PET that offers good surface appearance, high flow and good heat performance. EH7020HF was developped for automotiove bezel application that require basecoat +..
Flexural Modulus 4.68 GPa
679 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP DF0029P PC
LNP THERMOCOMP* DF0029P is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added features of this material include: Exceptional Processing. Flame Retardant.
Flexural Modulus 4.68 GPa
679 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP JF002 PES (Asia Pacific)
LNP THERMOCOMP* JF002 is a compound based on Polyethersulfone resin containing Glass Fiber.
Flexural Modulus 4.68 GPa
679 ksi
ASTM D 790
SABIC Innovative Plastics LNP Thermocomp JX89569 PES
LNP THERMOCOMP* JX89569 is a compound based on Polyethersulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 4.68 GPa
679 ksi
ASTM D 790
SABIC Innovative Plastics LNP Thermocomp JX89569 PES (Asia Pacific)
LNP* THERMOCOMP* JX89569 is a compound based on Polyethersulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.