Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.462 GPa @Temperature -40.0 °C |
67.0 ksi @Temperature -40.0 °F |
ASTM D790 |
Teknor Apex TEKRON® 4300-D90B Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Flexural Modulus | 0.462 - 0.600 GPa | 67.0 - 87.0 ksi | ASTM D790 |
Buckeye Polymers BP FLEX D0850(C) BLK Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |