Polymer Property : Flexural Modulus = 0.462 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.462 GPa

@Temperature -40.0 °C
67.0 ksi

@Temperature -40.0 °F
ASTM D790
Teknor Apex TEKRON® 4300-D90B Thermoplastic Elastomer
Information provided by Teknor Apex Company
Flexural Modulus 0.462 - 0.600 GPa
67.0 - 87.0 ksi
ASTM D790
Buckeye Polymers BP FLEX D0850(C) BLK Thermoplastic Polyolefin
Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist..