Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.61 GPa | 669 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP KF002 Acetal Copolymer LNP THERMOCOMP* KF002 is a compound based on Acetal Copolymer resin containing 10% Glass Fiber. |
|||
Flexural Modulus | 4.61 GPa | 669 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP KX97390 Acetal Copolymer LNP THERMOCOMP* KX97390 is a compound based on Acetal Copolymer resin containing Glass Fiber. Added features of this material include: Chemically Coupled. |
|||
Flexural Modulus | 4.61 GPa | 669 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP MX99432 PP LNP* THERMOCOMP* MX99432 is a compound based on Polypropylene resin containing Proprietary Filler(s). |
|||
Flexural Modulus | 4.61 GPa | 669 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RF002ES PA 66 LNP THERMOCOMP* RF002ES is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
Flexural Modulus | 4.61 GPa | 669 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP KF002XXP Acetal Copoly LNP* Thermocomp* KF002XXP is a compound based on Acetal Copolymer resin containing 10% Glass Fiber. Added features of this material include: Chemically Coupled. |
|||
Flexural Modulus | 4.61 GPa | 669 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP MX99432 PP (Asia Pacific) LNP* Thermocomp* MX99432 is a compound based on Polypropylene resin containing Glass Fiber. |