Mechanical Properties Metric English Comments
Flexural Modulus 6.69 GPa
970 ksi
1.3 mm/min; ASTM D790
PolyOne LubriOne™ PS-30GF/2S Natural Polybutylene Terephthalate (PBT)
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Flexural Modulus 6.69 GPa

@Temperature 23.0 °C
970 ksi

@Temperature 73.4 °F
ISO 178
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stabi..
Flexural Modulus 6.69 GPa

@Temperature 23.0 °C
970 ksi

@Temperature 73.4 °F
ISO 178
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA), 16% Glass Fiber (Dry)
Amodel® AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s..
Flexural Modulus 6.69 GPa
970 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP JF004 PES
LNP THERMOCOMP* JF004 is a compound based on Polyethersulfone resin containing 20% Glass Fiber.
Flexural Modulus 6.69 GPa
970 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP JF004 PES (Asia Pacific)
LNP* THERMOCOMP* JF004 is a compound based on Polyethersulfone resin containing Glass Fiber.
Flexural Modulus 6.69 GPa
970 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP JF004E PES (Asia Pacific)
LNP* Thermocomp* JF004E is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Easy Molding.
Flexural Modulus 6.69 GPa
970 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP JF004EXP PES
LNP* THERMOCOMP* JF004EXP is a compound based on Polyethersulfone resin containing 20% Glass Fiber. Added features of this material include: Easy Molding.
Flexural Modulus 6.69 GPa
970 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP JF004EXP PES (Asia Pacific)
LNP* Thermocomp* JF004EXP is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Easy Molding.
Flexural Modulus 6.69 GPa
970 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP JF004E PES
LNP* THERMOCOMP* JF004E is a compound based on Polyethersulfone resin containing 20% Glass Fiber. Added features of this material include: Easy Molding.