Mechanical Properties Metric English Comments
Flexural Modulus 6.08 GPa
882 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP DFI14 PC
LNP* Lubricomp* DFI14 is a compound based on Polycarbonate resin containing 20% Glass Fiber and 2% Silicone. Added features include: Internally Lubricated.
Flexural Modulus 6.08 GPa
882 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Valox® VIC4311 PBT
VALOX VIC4311 is a 30% glass filled, impact modified PBT with excellent epoxy adhesion. Automotive underhood applications such as ignition coil housings.
Flexural Modulus 6.08 GPa
882 ksi
ASTM D790
SABIC Innovative Plastics Valox® VIC4311 PBT (Asia Pacific)
Flexural Modulus 6.08 GPa
882 ksi
ASTM D790
Shinkong Synthetic Fibers Shinite® T102G15 PET, 15% Glass Filled, Fire Retardant
Information from Shinkong Synthetic Fibers Corp.
Flexural Modulus 6.08 GPa
882 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP AF004XXY ABS
LNP* Thermocomp* AF004XXY is a compound based on ABS containing 20% glass fiber.
Flexural Modulus 6.08 GPa
882 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP AX02749 ABS
LNP* THERMOCOMP* AX02749 is a compound based on ABS containing proprietary fillers.
Flexural Modulus 6.08 GPa
882 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP DF0049P PC
LNP* Thermocomp* DF0049P is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Exceptional Processing, Flame Retardant.
Flexural Modulus 6.08 GPa
882 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP IF004 PA6.12
LNP* THERMOCOMP* IF004 is a compound based on Nylon 6/12 resin containing 20% Glass Fiber.
Flexural Modulus 6.08 GPa
882 ksi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Infino® XI-4208 PA, Glass Filled
Information provided by Samsung Cheil Industries.
Flexural Modulus 6.08 GPa
882 ksi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Infino® XI-4208 PA, Glass Filled
Information provided by Samsung Cheil Industries.
Flexural Modulus 6.08 GPa
882 ksi
ASTM D790
Samyang Tribit® 1500GN15 Polybutylene Terephthalate, 15% Glass Reinforced, Flame Retardant
Characteristics:G/F reinforcedFlame retardantHeat and Impact resistantApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A..
Flexural Modulus 6.08 GPa
882 ksi
ASTM D790
SABIC Innovative Plastics NORYL NC212 PPE+HIPS (Asia Pacific)
Flexural Modulus 6.08 GPa
882 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP DF0049P PC (Asia Pacific)
LNP* Thermocomp* DF0049P is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Exceptional Processing, Flame Retardant.
Flexural Modulus 6.08 GPa
882 ksi
ASTM D790
PlastxWorld CEVIAN® EG506 ABS
Inherently Static Dissipative and Glass Fiber reinforced ABS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by Plastx..
Flexural Modulus 6.08 GPa
882 ksi
ASTM D790
E-Polymers TEKAMID® TB110SG30 30% Glass Fiber Reinforced, High Impact PA6 Resin
Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.T-series: Impact modified,..
Flexural Modulus 6.08 GPa
882 ksi
ASTM D790
SABIC Innovative Plastics NORYL PX2922 PPE (Asia Pacific)
GF20% FR-V0
Copyright © lookpolymers.com All Rights Reserved