Polymer Property : Flexural Modulus = 59.0 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.407 GPa
59.0 ksi
2% secant; ASTM D790
ExxonMobil LL 6202.19 Injection Molding Resin
Product Description: LL 6202 is a narrow molecular weight butane copolymer designed for applications that require excellent toughness. This resin offers easy processability for applications that req..
Flexural Modulus 0.407 GPa
59.0 ksi
2% Secant; ASTM D638
ExxonMobil LLDPE LL 6201.19 Linear Low Density Polyethylene Resin
Product Description: LL 6202 is a narrow molecular weight butane copolymer designed for applications that require excellent toughness. This resin offers easy processability for applications that req..
Flexural Modulus 0.407 GPa
59.0 ksi
2% Secant; ASTM D638
ExxonMobil LLDPE LL 6202.19 Linear Low Density Polyethylene Resin
Product Description: LL 6202 is a narrow molecular weight butane copolymer designed for applications that require excellent toughness. This resin offers easy processability for applications that req..