Mechanical Properties Metric English Comments
Flexural Modulus 4.05 GPa
587 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Xenoy® 1760 PBT+PC
11% Glass Reinforced PBT+PC alloy. Impact/chemical resistant. Excellent physical property retention in automotive exteriors.
Flexural Modulus 4.05 GPa
587 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Xenoy® X5630Q PC+PET (Europe-Africa-Middle East)
Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applications
Flexural Modulus 4.05 GPa
587 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP RB006 PA 66
LNP* THERMOCOMP* RB006 is a compound based on Nylon 66 resin containing 30% Glass Bead.
Flexural Modulus 4.05 GPa

@Temperature 23.0 °C
587 ksi

@Temperature 73.4 °F
EN ISO 178
Ensinger TECASINT™ 2021 Polyimide, 15% Graphite (PI)
TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications...
Flexural Modulus 4.05 GPa
587 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Xenoy® X5630P PET+PC (Europe-Africa-Middle East)
Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applications