Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.380 GPa | 55.1 ksi | ASTM D790 |
ICO Polymers ICORENEâ„¢ 110-1329 LMDPE Rotational Molding Resin Description: ICORENE 110-1329 is a linear medium density polyethylene developed for use in rotational molding. This is a very fast processing material that quickly molds out to offer low surface po.. |
|||
Flexural Modulus | 0.380 GPa | 55.1 ksi | 1.3 mm/min; ASTM D790 |
ICO Polymers ICORENEâ„¢ 115-1329 LMDPE Rotational Molding Resin Description: ICORENE 115-1329 is a linear medium density polyethylene developed for use in rotational molding. It is an easy processing material with good surface gloss, scratch resistance and gene.. |
|||
Flexural Modulus | 0.380 GPa | 55.1 ksi | 1.33 mm/min; ASTM D790 |
ICO Polymers ICORENEâ„¢ 190-1329 LMDPE Rotational Molding Resin Description: ICORENE 190-1329 is a compounded linear medium density polyethylene copolymer developed for rotational molding. It has a good balance of properties such as toughness, easy flow and sti.. |
|||
Flexural Modulus | 0.380 GPa | 55.1 ksi | ISO 178 |
Solvay TECHNYL® C 442 Black V PA6, Conditioned Description: Unreinforced polyamide PA6, high viscosity, with high flexibility and very high impact resistance even at low temperature, for extrusion.Available in: Europe Product Applications: It ha.. |
|||
Flexural Modulus | 0.380 GPa | 55.1 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP TX97446 PU LNP* LUBRICOMP* TX97446 is a compound based on Polyurethane containing Proprietary Fillers. Added feature of this material is: Wear Resistant. |
|||
Flexural Modulus | 0.380 GPa | 55.1 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM STM1500 PEI Copolymer Siloxane polyetherimide block copolymer. Wire and cable use. Strength and flexibility. |
|||
Flexural Modulus | 0.380 GPa | 55.1 ksi | cond; ISO 178 |
DSM Novamid® ST145 NAT PA6-I Impact Modified, Injection Molding |
|||
Flexural Modulus | 0.380 GPa | 55.1 ksi | |
Dow DOWLEX™ 2500 Linear Low Density Polyethylene, Narrow MW Distribution DOWLEX® 2500 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer excellent environmental stress crack resistance and tear strength with high impact strength. It.. |
|||
Flexural Modulus | 0.380 GPa | 55.1 ksi | ASTM D790 |
C.O.I.M. LARIPUR® LPR6650 Modified Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
Flexural Modulus | 0.380 GPa | 55.1 ksi | ASTM D790 |
Ashley Polymers Ashlene® 940H Nylon 11 A general purpose highly flexible natural Nylon 11 resin with UV stabilizers.Data provided by the manufacturer |
|||
Flexural Modulus | 0.380 GPa | 55.1 ksi | ASTM D790 |
Ashley Polymers Ashlene® D930H Nylon 12 A plasticized Nylon 12 offering improved flexibility with superior moisture and chemical resistance. Also UV and heat stabilized, available in natural and precolored. Any color other than natural .. |
|||
Flexural Modulus | 0.380 GPa | 55.1 ksi | ASTM D790 |
Ashley Polymers Ashlene® T940H Nylon 11 A general purpose, highly flexible Natural Nylon 11 resin with UV stabilizers.Data provided by the manufacturer |
|||
Flexural Modulus | 0.380 - 1.38 GPa | 55.1 - 200 ksi | Average value: 0.985 GPa Grade Count:11 |
Overview of materials for Nylon 11, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Flexural Modulus | 0.380 - 32.6 GPa | 55.1 - 4730 ksi | Average value: 6.74 GPa Grade Count:797 |
Overview of materials for Polyetherimide (PEI) This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat.. |