Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.60 - 3.70 GPa @Temperature -20.0 - -20.0 °C |
377 - 537 ksi @Temperature -4.00 - -4.00 °F |
Average value: 3.15 GPa Grade Count:2 |
Overview of materials for Polypropylene with 30% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are.. |
|||
Flexural Modulus | 1.30 - 3.70 GPa | 189 - 537 ksi | Average value: 2.81 GPa Grade Count:45 |
Overview of materials for Nylon 6, Cast This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Flexural Modulus | 0.993 - 3.70 GPa | 144 - 537 ksi | Average value: 2.95 GPa Grade Count:26 |
Overview of materials for Nylon 6, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria.. |