Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.519 GPa | 800.5 ksi | ISO 178 |
Azdel Plus C401-B01 40% Chopped Fiber Mat / PP Resin Matrix AZDEL® C401-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat contained within a polypropylene resin matrix. This composite material features high flow prope.. |