Material Notes:
AZDEL® C401-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat contained within a polypropylene resin matrix. This composite material features high flow properties and a very homogeneous fiber distribution. This material is typically used for standard semi-structural thin wall applications and where good glass distributions into features such as ribs and bosses is desired.Mechanical properties and mold shrinkage measured on flat plaques.Information provided by Azdel.
Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
1.17 g/cc
Laminate; ASTM D792
1.19 g/cc
1.19 g/cc
Molded; ASTM D792
Filler Content 40 %
40 %
By weight (ashing); Internal
Thickness 3600 microns
142 mil
Sheet; Internal
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
Measured on flat plaques; ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 105.7 MPa
15330 psi
ISO 527
Elongation at Break 2.2 %
2.2 %
ISO 527
Tensile Modulus 5.965 GPa
865.2 ksi
ISO 527
Flexural Strength 146 MPa
21200 psi
ISO 178
Flexural Modulus 5.519 GPa
800.5 ksi
ISO 178
Poissons Ratio 0.333
0.333
ISO 527
Izod Impact, Notched 4.69 J/cm

@Thickness 4.00 mm,
Temperature 23.0 °C
8.79 ft-lb/in

@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
Impact 254

@Thickness 4.00 mm
254

@Thickness 0.157 in
Multi-axial in kg, at max. load; ASTM D3763
Impact Test 10.0 J

@Thickness 4.00 mm
7.38 ft-lb

@Thickness 0.157 in
Multi-axial, at max. load; ASTM D3763
18.8 J

@Thickness 4.00 mm
13.9 ft-lb

@Thickness 0.157 in
Multi-axial, at failure; ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
ASTM D648
Flame Spread 4.5 mm/min
0.18 in/min
FMVSS302
Descriptive Properties Value Comments
Color Black
Internal