Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.14 - 5.10 GPa | 165 - 740 ksi | Average value: 2.06 GPa Grade Count:118 |
Overview of materials for Polycarbonate/PET Polyester Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values.. |