Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 33.103 GPa | 4801.2 ksi | ASTM D-790 |
PlastiComp Complet® LCF50 - TPU Rigid Thermoplastic Polyurethane, 50% Long Carbon Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 50% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |