Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.30 GPa | 478 ksi | ASTM D790 |
Entec Hyrene® PSCRY 2.5 General Purpose Polystyrene Available in North America Features: Crystal, General Purpose, and High Heat ResistanceRoHS Compliant Form: Pellets Information provided by Entec |