Mechanical Properties Metric English Comments
Flexural Modulus 3.29 GPa
477 ksi
ASTM D790
Omni Plastics OmniLon™ 6 PA6 WF10 Mineral Filled Nylon
Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics
Flexural Modulus 3.29 GPa
477 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP RAL22I PA 66
LNP* LUBRICOMP* RAL22I is a compound based on Nylon 66 resin containing 10% PTFE, 10% Aramid Fiber. Added features of this material include: Wear Resistant, High Impact.
Flexural Modulus 3.29 GPa

@Temperature 65.0 °C
477 ksi

@Temperature 149 °F
ASTM Test
BASF Ultramid® 8333G HI 33% Glass Filled PA6 (Conditioned)
Ultramid 8333G HI is a 14% glass reinforced, impact modified PA6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a balance of st..