Mechanical Properties Metric English Comments
Flexural Modulus 3.285 GPa
476.5 ksi
ASTM D790
Daelim H&L Plavis-MS DF MoS2 Filled Aromatic Polyimide Bearing
Direct Formed. Plavis-MS: MoS2 15 wt% filled, Self lubricating grade for vacuum environments.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 carbons is the criti..