Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.285 GPa | 476.5 ksi | ASTM D790 |
Daelim H&L Plavis-MS DF MoS2 Filled Aromatic Polyimide Bearing Direct Formed. Plavis-MS: MoS2 15 wt% filled, Self lubricating grade for vacuum environments.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 carbons is the criti.. |