Polymer Property : Flexural Modulus = 463 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 3.19 GPa
463 ksi
ASTM D790
PolyOne Geon™ Vinyl Rigid Extrusion 87345 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Flexural Modulus 3.19 GPa
463 ksi
ASTM D790
PolyOne Geon™ Vinyl Rigid Extrusion 87570 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Flexural Modulus 3.19 GPa
463 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® BFL2010 PC
Non-brominated, non-chlorinated flame retardant, glass reinforced PC with improved flow. Available in opaque colors.
Flexural Modulus 3.19 GPa
463 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® BFL2010 PC (Asia Pacific)
Non-brominated, non-chlorinated flame retardant, glass reinforced PC with improved flow. Available in opaque colors.
Flexural Modulus 3.19 GPa
463 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® BFL2010 PC (Europe-Africa-Middle East)
Non-brominated, non-chlorinated flame retardant, glass reinforced PC with improved flow. Available in opaque colors.
Flexural Modulus 3.19 GPa
463 ksi
ASTM D790
Entec Hyrene® PSCRY 1.5 General Purpose Polystyrene
Available in North America Features: Crystal, High Heat Resistance, General Purpose, High Molecular WeightRoHS Compliant Form: Pellets Information provided by Entec