Mechanical Properties Metric English Comments
Flexural Modulus 2.16 - 3.14 GPa
313 - 455 ksi
Average value: 2.63 GPa Grade Count:6
Overview of materials for PEN-PET
This property data is a summary of similar materials in the MatWeb database for the category "PEN-PET". Each property range of values reported is minimum and maximum values of appropriate MatWeb ent..