Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.100 GPa | 449.6 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylex® P1010G7FRMA Polycarbonate, 7% Glass Filled Polycarbonate, 7% Glass Filled, Flame RetardantInformation provided by Ravago. |