Mechanical Properties Metric English Comments
Flexural Modulus 3.100 GPa
449.6 ksi
ASTM D790
Ravago Manufacturing Americas Hylex® P1010G7FRMA Polycarbonate, 7% Glass Filled
Polycarbonate, 7% Glass Filled, Flame RetardantInformation provided by Ravago.