Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.989 GPa | 433.5 ksi | ASTM D790 |
Kleerdex Kydex® P90 Acrylic/PVC Extrusion Compound
(discontinued **) Low heat release aviation gradeApplications: Kydex P90 is designed for extrusion of profiles which need to meet the highest flammability requirement of PAR 25.853a for vertical burn, rate of heat re.. |