Mechanical Properties Metric English Comments
Flexural Modulus 2.92 GPa
424 ksi
ASTM D790
PolyOne Geon™ Vinyl Rigid Extrusion 87560 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Flexural Modulus 2.92 GPa
424 ksi
ASTM D790
PolyOne Geon™ Vinyl Rigid Extrusion 87707 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Flexural Modulus 2.92 GPa
424 ksi
ASTM D790
PolyOne Geon™ Vinyl Rigid Extrusion 87717 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Flexural Modulus 2.92 GPa
424 ksi
ASTM D790
PolyOne Geon™ Vinyl Rigid Extrusion 87727 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Flexural Modulus 2.92 GPa
424 ksi
ASTM D790
PolyOne Geon™ Vinyl Rigid Extrusion 87727-0284 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples. Physical property testing was based on the Geon® 87727 Trans 0020.Information provided by PolyOne
Flexural Modulus 2.92 GPa
424 ksi
ASTM D790
PolyOne Geon™ Vinyl Rigid Extrusion L9630 Polyvinyl Chloride, Rigid (PVC, Rigid)
Product can meet UL-94V-0. Material passed V-0 @ 1.5mm in screening test at PDI.Information provided by PolyOne
Flexural Modulus 2.92 GPa
424 ksi
ASTM D790
PolyOne Geon™ SF M7100 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Flexural Modulus 2.92 GPa
424 ksi
ASTM D790
PolyOne Geon™ SF M7120 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Flexural Modulus 2.92 GPa
424 ksi
ISO 178
SABIC Innovative Plastics LNP COLORCOMP JX91550 PES
LNP COLORCOMP* JX91550 is an unfilled Polyethersulfone.
Flexural Modulus 2.92 GPa
424 ksi
ISO 178
SABIC Innovative Plastics LNP COLORCOMP JX91550 PES (Asia Pacific)
LNP COLORCOMP* JX91550 is a compound based on Polyethersulfone resin containing Unfilled Custom Color.
Flexural Modulus 2.92 GPa
424 ksi
ASTM D790
Nilit Polynil® P50FIL Super Fast Cycling, Nucleated Nylon 66
Description: Polynil P50 FIL is a nucleated, internally lubricated NYLON 66 with excellent flow characteristics and very fast cycle time. It is widely used throughout many industries for mass produc..
Flexural Modulus 2.92 GPa
424 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP STAT-KON 9X02785 PC
LNP STAT-KON* 9X02785 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
Flexural Modulus 2.92 GPa
424 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics ULTEM 9085 PEI Blend
High flow Polyetherimide blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke and flame evolution.
Flexural Modulus 2.92 GPa
424 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics ULTEM 9085 PEI Blend (Asia Pacific)
High flow Polyetherimide blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke and flame evolution.
Flexural Modulus 2.92 GPa
424 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics ULTEM 9085 PEI Blend (Europe-Africa-Middle East)
High flow Polyetherimide blend. Meets FAR 25.853 and OSU 55/55 with low toxicity, smoke and flame evolution.