Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.76 - 2.90 GPa
400 - 421 ksi
ASTM D790
Proto3000 Accura® 45HC Plastic Stereolithography (SLA) Prototyping Polymer
A high speed material, with excellent thermal and moisture resistance for producing functional prototypes in 3D Systems' SLA 250 systems.Benefits:Fast build speed:Provides build speeds that are sign..
Flexural Modulus 2.07 - 2.90 GPa
300 - 421 ksi
ASTM D790
Novatec Novacycle® 501 PVC
Novacycle® 501 is a general purpose, rigid, extrusion grade PVC compound in pellet form. This formulation is designed to provide an economical alternative for extruded profiles Raw material appe..
Flexural Modulus 2.00 - 2.90 GPa
290 - 421 ksi
Average value: 2.54 GPa Grade Count:5
Overview of materials for Polycarbonate/Styrenic Alloy
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Styrenic Alloy". Each property range of values reported is minimum and maximum values of a..
Flexural Modulus 2.76 - 2.90 GPa
400 - 421 ksi
ASTM D790
3D Systems Accura® 45HC Plastic for SLA® Systems
A high speed material, with excellent thermal and moisture resistance for producing functional prototypes in 3D Systems' SLA 250 systems.ApplicationsHigh temperature testing:Automotive "under-the-ho..