Polymer Property : Flexural Modulus = 42.9 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.296 GPa
42.9 ksi
13 mm/min; ASTM D790
PolyOne Maxxam™ FR WC-P85 NHFR RoHS Natural Polyolefin, Unspecified
Maxxam™ HFFR WC-P85 RoHS Natural is a halogen-free flame retardant polyolefin compound characterized by low smoke, low flame spread, excellent spring-back, no plate-out and high extrusion line spee..
Flexural Modulus 0.296 GPa
42.9 ksi
0.01; ASTM D790
NOVA Chemicals Novapol® LA-0219-A LDPE Foam Resin
Features: Good heat sealing latitudeModerate toughnessEasy processability Applications: Industrial packagingLinersBlends with LLDPEFoam ArticlesInformation provided by Nova Chemicals
Flexural Modulus 0.296 GPa
42.9 ksi
at 1%; ASTM D790
NOVA Chemicals Novapol® LA-0219-AM LDPE Foam Resin
Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Industrial packaging, Liners, Blends with LLDPE, Foam articlesAdditives: Base resinFilm properties are typical of blo..