Mechanical Properties Metric English Comments
Flexural Modulus 2.86 GPa
415 ksi
ASTM D790
Nylene® 7139 (HS) Low Wear Nylon 6/6
Description: Nylene® 7139 (HS) is a general purpose, low wear, 1% MoS2 reinforced nylon 6/6. Information provided by Custom Resins.ALM, Nylene Canada, and Custom Resins are all operting companies o..
Flexural Modulus 2.86 GPa
415 ksi
ASTM D790
Nylene® PA6/6 Homopolymer 132 HSL Nylon 6/6
Low Viscosity GP Grade; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Flexural Modulus 2.86 GPa
415 ksi
ASTM D790
Polymer Resources PPX-MF-FR1 Modified-PPO, V-0 Flame Retardant, Mineral Reinforced
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDT, Mineral ReinforcedFeatures: • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mecha..
Flexural Modulus 2.86 GPa

@Thickness 3.17 mm
415 ksi

@Thickness 0.125 in
ASTM D790
PTS PCA-30G11-(V) UV Stabilized, Glass Reinforced PC/PBT Alloy
Information provided by Polymer Technology and Services, LLC (PTS).
Flexural Modulus 2.86 GPa
415 ksi
Tangent; ASTM D790
RheTech Products HP525-01 30% Talc Reinforced High Performance Polypropylene, UV Stabilized, Black
Applications: Center consolesInterior trimInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 2.86 GPa
415 ksi
Tangent; ASTM D790
RheTech Products HP525-283 30% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, RK8 Medium Camel
Applications: Automotive interior applicationsFan shroudsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 2.86 GPa

@Thickness 3.20 mm
415 ksi

@Thickness 0.126 in
15mm/min; ASTM D790
LG Chemical HIPS MI730 PS, Impact Modified
Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica..
Flexural Modulus 2.86 GPa

@Thickness 3.20 mm
415 ksi

@Thickness 0.126 in
15mm/min; ASTM D790
LG Chemical HIPS MI750L PS, Impact Modified
Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica..
Flexural Modulus 2.86 GPa
415 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Lubricomp RL001 PA 66
LNP Lubricomp* RL001 is a Nylon 6/6 base resin containing PTFE lubricant. Characteristics are internally lubricated.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 2.86 GPa
415 ksi
ASTM D790
Teknor Apex Chemlon® 100 Nylon 66, Unreinforced
Features: Basic nylon 66 with internal lubrication. Widely used for automotive, electronic and appliance applications. Processing Method: Injection Molding Forms: Pellets Automotive Specifications: ..
Flexural Modulus 2.86 GPa
415 ksi
ASTM D790
Teknor Apex Chemlon® 212 Nylon 6, Unreinforced
Features: Lubricated, General Purpose; General purpose nylon 6; Slightly tougher and more ductile than nylon 66 Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex..
Flexural Modulus 2.86 GPa
415 ksi
ASTM D790
Chase Plastics CP Pryme® AH300 Acetal Homopolymer, Recycled Content
Features: General purposeHigh heat resistanceGood chemical resistanceGood dimensional stabilityFatigue resistantLow frictionGrease resistantLow moisture absorptionOil resistantHigh rigiditySolvent r..
Flexural Modulus 2.86 GPa
415 ksi
ASTM D790
Chase Plastics CP Pryme® NN300HSL (DAM) Nylon 66 (Utility Grade), Heat Stabilized, Internally Lubricated
Information provided by Chase Plastics.
Flexural Modulus 2.86 GPa
415 ksi
ASTM D790
Chase Plastics CP Pryme® NN300L (DAM) Nylon 66 (Utility Grade), Internally Lubricated
Information provided by Chase Plastics.
Flexural Modulus 2.86 GPa
415 ksi
ISO 178
Hexcel® HexPly® M18 356°F (180°C) Curing Epoxy Matrix
HexPly® M18 has been developed to fulfill the requirements of the aerospace industry for primary structures using standard manufacturing processes. The matrix has improved properties which allow ea..
Flexural Modulus 2.86 GPa
415 ksi
ASTM D790
Diamond Polymers NYLON 66 Natural
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Flexural Modulus 2.86 GPa
415 ksi
ISO Data
BASF Ultrason E 2010 PES
Ultrason E 2010 is an unreinforced, medium viscosity standard injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability. It conforms to FDA req..
Flexural Modulus 2.86 GPa
415 ksi
ASTM D790
Polymer Resources PPX-MF-FR1 Modified PPO, UL 94 V-0 with HDT of 190 F, Mineral Reinforced  (Unverified Da
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Flexural Modulus 2.86 GPa
415 ksi
Tangent; ASTM D790
RheTech Products F24-01 20% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: Head lamp housingsBracketsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.