Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.283 GPa | 41.0 ksi | 2% Secant, 12.7 mm/min; ASTM D790 |
Eastman E6838-913P Polyethylene
(discontinued **) Polyethylene E6838-913P natural is a specialty formulation suggested for high-speed extrusion coating applications. E6838-913P offers improvements over standard low-density polyethylene in adhesion .. |