Polymer Property : Flexural Modulus = 0.283 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.283 GPa
41.0 ksi
2% Secant, 12.7 mm/min; ASTM D790
Eastman E6838-913P Polyethylene  (discontinued **)
Polyethylene E6838-913P natural is a specialty formulation suggested for high-speed extrusion coating applications. E6838-913P offers improvements over standard low-density polyethylene in adhesion ..