Mechanical Properties Metric English Comments
Flexural Modulus 4.71 GPa

@Thickness 3.20 mm
683 ksi

@Thickness 0.126 in
1.3mm/min; ASTM D790
LG Chemical LUMID GP2130A(W) PA6+GF13%, General Purpose
Feature: Injection Molding, PA6+GF13%, General PurposeApplication: Automotive PartsCAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical
Flexural Modulus 4.71 GPa
683 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® EH7020HF PBT+PET
Valox EH7020HF is a mineral filled PBT/PET that offers good surface appearance, high flow and good heat performance. EH7020HF was developed for automotive bezel application that requires basecoat + ..
Flexural Modulus 4.71 GPa
683 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® EH7020HF PBT+PET (Asia Pacific)
Valox EH7020HF is a mineral filled PBT/PET that offers good surface appearance, high flow and good heat performance. EH7020HF was developped for automotiove bezel application that require basecoat +..
Flexural Modulus 4.71 GPa
683 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Thermocomp GF003 PSU
LNP THERMOCOMP* GF003 is a compound based on Polysulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 4.71 GPa
683 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Thermocomp ZZ006 PPE+PS
LNP THERMOCOMP* ZZ006 is a compound based on PPE+PS Blend resin containing Milled Glass.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 4.71 GPa
683 ksi
ISO 178
Polyplastics Duranex® 3116 Polybutylene Terephthalate (PBT), Standard, FR, UL approved regrind 50%, 7.5% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Flexural Modulus 4.71 GPa
683 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOTUF WF003I Polyester, TP
LNP THERMOTUF* WF003I is a compound based on Polyester, TP resin containing Glass Fiber. Added features of this material include: High Impact.