Polymer Property : Flexural Modulus = 4.44 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 4.44 GPa
644 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Thermocomp DFZ22E PC
LNP* Thermocomp* DFZ22E is a compound based on Polycarbonate with Glass and Milled Fiber. Characteristics of this products is Easy Molding.This data was supplied by SABIC-IP for the Americas region..
Flexural Modulus 4.44 GPa
644 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Thermocomp RX06324 PA 66 (Asia Pacific)
This material is Mineral filled Nylon grade with high dielectric constantThis data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Modulus 4.44 GPa
644 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 (Asia Pacific)
Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al..
Flexural Modulus 4.44 GPa
644 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6
Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al..
Flexural Modulus 4.44 GPa
644 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 (Europe-Africa-Middle East)
Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al..
Flexural Modulus 4.44 GPa

@Temperature 23.0 °C
644 ksi

@Temperature 73.4 °F
EN ISO 178
Ensinger TECASINT 4201 SD Polyimide, Black, Carbon Fiber (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..