Polymer Property : Flexural Modulus = 4.395 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 4.395 GPa
637.4 ksi
ISO 178
A. Schulman SCHULAMID® 6 GB30 30% Glass Bead Reinforced Nylon 6
Information provided by A. Schulman.
Flexural Modulus 4.395 GPa
637.4 ksi
ISO 178
A. Schulman SCHULAMID® 6 GB30 30% Glass Bead Reinforced Nylon 6
Information provided by A. Schulman.
Flexural Modulus 4.395 GPa
637.4 ksi
ISO 178
A. Schulman SCHULAMID® 6 GB30 30% Glass Bead Reinforced Nylon 6
Information provided by A. Schulman.
Flexural Modulus 4.395 GPa
637.4 ksi
ISO 178
A. Schulman SCHULAMID® 6 GB30 30% Glass Bead Reinforced Nylon 6
Information provided by A. Schulman.
Flexural Modulus 4.395 GPa
637.4 ksi
ISO 178
A. Schulman SCHULAMID® 6 GB30 30% Glass Bead Reinforced Nylon 6
Information provided by A. Schulman.
Flexural Modulus 4.395 GPa
637.4 ksi
ISO 178
A. Schulman SCHULAMID® 6 GB30 30% Glass Bead Reinforced Nylon 6
Information provided by A. Schulman.