Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.364 GPa | 632.9 ksi | X direction, Condition A; ASTM D790 |
Rogers Corporation RT/duroid® 6010.2LM Ceramic-PTFE Composite Microwave Laminate Features:High dielectric constant for circuit size reductionLow loss - Ideal for operating at X-band or belowLow Z-axis expansion. Provides reliable plated through holes in multi-layer boardsTight .. |