Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 26.59 GPa | 3857 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP UC008H PPA LNP THERMOCOMP* UC008H is a compound based on Polyphthalamide resin containing 40% Carbon Fiber. Added features of this material include: Electrically Conductive, Healthcare. |
|||
Flexural Modulus | 26.59 GPa | 3857 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP UC008H PPA (Asia Pacific) LNP* THERMOCOMP* UC008H is a compound based on Polyphthalamide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 26.59 GPa | 3857 ksi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp UC008S PPA (Asia Pacific) LNP* Thermocomp* UC008S is a compound based on Polyphthalamide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for.. |
|||
Flexural Modulus | 26.59 GPa | 3857 ksi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp UC008S PPA LNP* Thermocomp* UC008S is a compound based on Polyphthalamide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for.. |