Polymer Property : Flexural Modulus = 26.59 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 26.59 GPa
3857 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP UC008H PPA
LNP THERMOCOMP* UC008H is a compound based on Polyphthalamide resin containing 40% Carbon Fiber. Added features of this material include: Electrically Conductive, Healthcare.
Flexural Modulus 26.59 GPa
3857 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP UC008H PPA (Asia Pacific)
LNP* THERMOCOMP* UC008H is a compound based on Polyphthalamide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Flexural Modulus 26.59 GPa
3857 ksi
ISO 178
SABIC Innovative Plastics LNP Thermocomp UC008S PPA (Asia Pacific)
LNP* Thermocomp* UC008S is a compound based on Polyphthalamide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for..
Flexural Modulus 26.59 GPa
3857 ksi
ISO 178
SABIC Innovative Plastics LNP Thermocomp UC008S PPA
LNP* Thermocomp* UC008S is a compound based on Polyphthalamide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for..