Polymer Property : Flexural Modulus = 3812.0 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 26.283 GPa
3812.0 ksi
ASTM D-790
PlastiComp Complet® LCF30-PC/ABS Polycarbonate/ABS Alloy, 30% Long Carbon Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polycarbonate/ABS Alloy with 30% long carbon fiber reinforcementInformation provided b..