Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 26.283 GPa | 3812.0 ksi | ASTM D-790 |
PlastiComp Complet® LCF30-PC/ABS Polycarbonate/ABS Alloy, 30% Long Carbon Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polycarbonate/ABS Alloy with 30% long carbon fiber reinforcementInformation provided b.. |