Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.469 GPa | 358.1 ksi | ASTM D790 |
Lucent Polymers PC/PBT-1430U Polycarbonate+PBT, Superior Weatherability, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |