Polymer Property : Flexural Modulus = 2.469 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.469 GPa
358.1 ksi
ASTM D790
Lucent Polymers PC/PBT-1430U Polycarbonate+PBT, Superior Weatherability, Injection Grade
Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc.