Polymer Property : Flexural Modulus = 355 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.40 - 2.45 GPa
348 - 355 ksi
ASTM D790M
DSM Somos® ProtoGen™ O-XT 18120 Epoxy Resin for Stereolithography, UV Postcure at HOC +3
DescriptionDSM Somos® ProtoGen O-XT 18120 is a liquid photopolymer that produces accurate parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demonstrate diffe..
Flexural Modulus 2.40 - 2.45 GPa
348 - 355 ksi
ASTM D790M
DSM Somos® ProtoGen™ O-XT 18420 Epoxy Resin for Stereolithography, UV Postcure at HOC +3
DescriptionDSM Somos® ProtoGen O-XT 18420 is a liquid, ABS-like, photopolymer that produces accurate parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demons..
Flexural Modulus 1.65 - 2.45 GPa
240 - 355 ksi
Average value: 2.08 GPa Grade Count:7
Overview of materials for Acrylic, Gamma Radiation Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Gamma Radiation Resistant, Molded". Each property range of values reported is minimum and maxim..
Flexural Modulus 0.689 - 2.45 GPa
99.9 - 355 ksi
Average value: 1.19 GPa Grade Count:65
Overview of materials for Polypropylene, Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Blow Molding Grade". Each property range of values reported is minimum and maximum values..