Mechanical Properties Metric English Comments
Flexural Modulus 2.43 GPa
353 ksi
ASTM D790
Teknor Apex APEX® RS 9011A Polyvinyl Chloride, Rigid
Forms: PelletsInformation Provided by Teknor Apex
Flexural Modulus 2.43 GPa
353 ksi
Tangent, chs 0.05 in/min; ASTM D790
Diamond Polymers ABS 1501
Description: Injection Molding GradeInformation provided by Diamond Polymers, Inc.
Flexural Modulus 2.43 GPa
353 ksi
Tangent, chs 0.05 in/min; ASTM D790
Diamond Polymers ABS 1501E
Description: Extrusion GradeInformation provided by Diamond Polymers, Inc.
Flexural Modulus 2.43 GPa
353 ksi
Tangent, chs 0.05 in/min; ASTM D790
Diamond Polymers ABS 1502
Description: Injection Molding Grade, High GlossInformation provided by Diamond Polymers, Inc.
Flexural Modulus 2.43 GPa
353 ksi
Tangent, chs 0.05 in/min; ASTM D790
Diamond Polymers ABS 7501 E
Description: Extrusion Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc.
Flexural Modulus 2.43 GPa
353 ksi
Tangent, chs 0.05 in/min; ASTM D790
Diamond Polymers ASA TW-18B2
Description: ASA Weatherable Polymer, Injection Molding Grade, Very High HeatInformation provided by Diamond Polymers, Inc.
Copyright © lookpolymers.com All Rights Reserved