Teknor Apex APEX® RS 9011A Polyvinyl Chloride, Rigid

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade
Manufacturer Teknor Apex Company
Trade Name APEX®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex APEX® RS 9011A Polyvinyl Chloride, Rigid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Forms: PelletsInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.42 g/cc
1.42 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 83
83
10 seconds; ASTM D2240
Tensile Modulus 2.38 GPa
345 ksi
ASTM D638
Flexural Modulus 2.43 GPa
353 ksi
ASTM D790
Izod Impact, Notched 2.56 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
4.80 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
Compression Molded; ASTM D256
Dart Drop Total Energy 147 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
0.276 ft-lb/mil

@Thickness 0.125 in,
Temperature 73.0 °F
Procedure A, 0.125" Conical Dart
Descriptive Properties Value Comments
Appearance Opaque