Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.303 GPa | 334.0 ksi | Method 1, Proc. B; ASTM D-790-95 |
Multibase Multi-Pro® 2005 T BLK Polypropylene PP compound suitable for automotive applications, meets elevated temperature resistance. Meets ESH-M4D-293-B specifications.Data provided by Multibase. |
|||
Flexural Modulus | 2.303 GPa | 334.0 ksi | ASTM D790 |
Kolon KOCETAL® K300HRD Wear Modified Acetal Resin Improved weather resistant grade suitable for out door use. Applications: Weather resistant products. Information provided by API-Kolon. |