PP compound suitable for automotive applications, meets elevated temperature resistance. Meets ESH-M4D-293-B specifications.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792-91
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
ASTM D955-89
Melt Flow 5.0 g/10 min
5.0 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Hardness, Shore D 73
73
10 sec; ASTM D-2240-95
Tensile Strength, Ultimate 31.0 MPa
4500 psi
ASTM D638-95
Elongation at Break 60 %
60 %
ASTM D638-95
Flexural Modulus 2.303 GPa
334.0 ksi
Method 1, Proc. B; ASTM D-790-95
Izod Impact, Notched 0.370 J/cm
0.693 ft-lb/in
ASTM D256-93a
Gardner Impact 0.700 J
0.516 ft-lb
ASTM D5420-93
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 107 °C
225 °F
ASTM D648-95
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ASTM D648-95