Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.896 - 2.30 GPa | 130 - 334 ksi | Average value: 1.52 GPa Grade Count:39 |
Overview of materials for Polypropylene, Sheet/Thermoforming Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Sheet/Thermoforming Grade". Each property range of values reported is minimum and maximum.. |