Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 21.62 GPa | 3136 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Stat-kon OEL36A PPS LNP* Stat-Kon* OEL36A is a compound based on Polyphenylene Sulfide resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This .. |
|||
Flexural Modulus | 21.62 GPa | 3136 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON OEL36A PPS - BRANCHED LNP* STAT-KON* OEL36A is a compound based on PPS - Branched resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive. |