Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.156 GPa | 312.7 ksi | ASTM D790 |
Kolon KOCETAL® LW301 Wear Modified Acetal Resin Special polymer added, improved wear property. Applications: Products for low noise and precision gear. Information provided by API-Kolon. |
|||
Flexural Modulus | 2.156 GPa | 312.7 ksi | ASTM D790 |
Kolon KOCETAL® MS301 Wear Modified Acetal Resin Molybdenum disulfide added, improved wear property. Applications: Products for low noise and friction against metal. Information provided by API-Kolon. |
|||
Flexural Modulus | 2.156 GPa | 312.7 ksi | ASTM D790 |
Kolon KOCETAL® SO301 Wear Modified Acetal Resin Silicone Oil added, improved wear property. Information provided by API-Kolon. |
|||
Flexural Modulus | 2.156 GPa | 312.7 ksi | ASTM D790 |
Kolon KOCETAL® VT301 Anti-Static Grade Acetal Resin Improved antistatic effects. Applications: Products for avoiding electric contamination. Information provided by API-Kolon. |