Mechanical Properties Metric English Comments
Flexural Modulus 2.156 GPa
312.7 ksi
ASTM D790
Kolon KOCETAL® LW301 Wear Modified Acetal Resin
Special polymer added, improved wear property. Applications: Products for low noise and precision gear. Information provided by API-Kolon.
Flexural Modulus 2.156 GPa
312.7 ksi
ASTM D790
Kolon KOCETAL® MS301 Wear Modified Acetal Resin
Molybdenum disulfide added, improved wear property. Applications: Products for low noise and friction against metal. Information provided by API-Kolon.
Flexural Modulus 2.156 GPa
312.7 ksi
ASTM D790
Kolon KOCETAL® SO301 Wear Modified Acetal Resin
Silicone Oil added, improved wear property. Information provided by API-Kolon.
Flexural Modulus 2.156 GPa
312.7 ksi
ASTM D790
Kolon KOCETAL® VT301 Anti-Static Grade Acetal Resin
Improved antistatic effects. Applications: Products for avoiding electric contamination. Information provided by API-Kolon.