Mechanical Properties Metric English Comments
Flexural Modulus 21.3 GPa
3090 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP OCL36 PPS - Linear (Europe-Africa-Middle East)
LNP* Lubricomp* OCL4036L is a compound based on PPS - Linear resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive.
Flexural Modulus 21.3 GPa
3090 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP OCL36A PPS - Branched (Europe-Africa-Middle East)
LNP* Lubricomp* OCL4036 is a compound based on PPS - Branched resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive.
Flexural Modulus 21.3 GPa
3090 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP OCL36XXP PPS - Linear (Europe-Africa-Middle East)
LNP* LUBRICOMP* OCL36XXP is a compound based on PPS- Linear resin containing PTFE, Carbon Fiber. Added features include : Internally Lubricated, Electrically Conductive .
Flexural Modulus 21.3 GPa
3090 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP OCP36 PPS
LNP* LUBRICOMP* OCP36 is a compound based on Polyphenylene Sulfide resin containing 30% Carbon Fiber, 15% PTFE/Silicone. Added features of this grade include: Wear Resistant, Bearing Grade, Electr..
Flexural Modulus 21.3 GPa
3090 ksi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP RCP36 PA 66
LNP LUBRICOMP* RCP36 is a compound based on Nylon 66 resin containing 30% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear Resistant.
Flexural Modulus 21.3 GPa
3090 ksi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP RCP36 PA 66 (Asia Pacific)
LNP LUBRICOMP* RCP36 is a compound based on Nylon 66 resin containing Silicone, PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive.
Flexural Modulus 21.3 GPa
3090 ksi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP RCP36 PA 66 (Europe-Africa-Middle East)
LNP LUBRICOMP* RCP36 is a compound based on Nylon 66 resin containing Carbon Fiber, Silicone, PTFE. Added features of this material include: Electrically Conductive.
Flexural Modulus 21.3 GPa
3090 ksi
ISO 178
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber
AvaSpire® AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621..
Flexural Modulus 21.3 GPa
3090 ksi
ISO 178
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621 CF30 gr..